We recommend using EPAMOULD 175 A 56 for injection molding processes, such as production of technical parts and footwear components. .
| Property | Norm | Value | Unit |
|---|---|---|---|
| Density | ASTM D 792 | 1,20 | g/cm³ |
| Hardness (5 sec.) | ASTM D 2240 | 79 | Shore A |
| Tensile strength | ASTM D 412 | 30 | psi psi |
| Elongation @ break | ASTM D 412 | 700 | % % |
| Tear strength | ASTM D 624 | 75 | pli pli |
| Abrasion | ISO 4649 | 60 | mm³ |
Values shown are based on testing of laboratory test specimens, conditioned at 70°C for 14 hours, and represent data that fall within the standard range of properties for the natural material. They are not intended for use in establishing maxiumum, minimum or range of values for specification purpose.